Call Us Today! +8613615170334 | jordangoldman92@gmail.com
Vacuum Ceramic Filter Press for Mining & Dewatering | Efficient Solid-Liquid Separation Equipment
Filtering area: 4-150㎡
Tank volume: 0.21-24m³
Power: 2.0-47kw
Contact with our professionals
Vacuum Ceramic Filter Press integrates electromechanical, microporous ceramics and ultrasonic technology, and is a new type of high-efficiency and energy-saving filtration equipment that relies on vacuum suction and capillary action to achieve solid-liquid separation. It is widely used in mining, metallurgy, chemical industry, environmental protection and other industries.
High vacuum (-0.09~-0.089)MPa), low moisture of filter cake. The solid content of filtrate is <50ppm, which can be used repeatedly and reduce emissions. Compared with traditional filtration equipment, the energy consumption is more than 90%, low energy consumption and low running cost. Compared with the traditional ceramic filter, it has increased the cake washing, which is suitable for the materials to be washed. High degree of automation, reduce labour intensity. Compact structure, small footprint, convenient installation and maintenance.
Adopting advanced liquid discharge system, it can be used under any working conditions.




| Machine specification ㎡ | Filter plate specification ㎡ | Quantity of discs | Quantity of filter plates | Filtration area ㎡ | Installed power Kw | Operating power Kw | Weight kg | Length mm | Width mm | Height mm |
|---|---|---|---|---|---|---|---|---|---|---|
| 4 | 2 | 2 | 24 | 4 | 7.60 | 6.60 | 2000 | 2460 | 2480 | 2100 |
| 8 | 2 | 4 | 48 | 8 | 8.80 | 7.40 | 3000 | 2960 | 2800 | 2100 |
| 12 | 3 | 4 | 48 | 12 | 9.20 | 7.40 | 5000 | 3200 | 3080 | 2450 |
| 15 | 3 | 5 | 60 | 15 | 12.10 | 9.90 | 5500 | 4300 | 3100 | 2490 |
| 18 | 3 | 6 | 72 | 18 | 12.50 | 9.90 | 6000 | 4600 | 3100 | 2490 |
| 21 | 3 | 7 | 84 | 21 | 12.90 | 9.90 | 6500 | 4900 | 3100 | 2490 |
| 24 | 3 | 8 | 96 | 24 | 15.80 | 12.40 | 7500 | 5200 | 3170 | 2530 |
| 30 | 3 | 10 | 120 | 30 | 19.75 | 15.55 | 9000 | 5800 | 3170 | 2530 |
| 36 | 4 | 9 | 108 | 36 | 22.85 | 19.05 | 9700 | 5110 | 3435 | 2820 |
| 40 | 5 | 8 | 96 | 40 | 24.85 | 19.85 | 11500 | 4870 | 3450 | 2900 |
| 45 | 5 | 9 | 108 | 45 | 25.45 | 19.85 | 11500 | 5170 | 3450 | 2900 |
| 60 | 5 | 12 | 144 | 60 | 35.40 | 28.00 | 13800 | 6600 | 3450 | 2900 |
| 80 | 5 | 16 | 192 | 80 | 49.00 | 39.99 | 18500 | 7990 | 3720 | 2900 |
| 100 | 5 | 20 | 240 | 100 | 63.90 | 51.50 | 21500 | 9190 | 3720 | 2960 |
| 120 | 6 | 20 | 240 | 120 | 81.90 | 67.50 | 24500 | 9190 | 3850 | 3180 |
| Mineral types | Particle size distribution | Range concentration % | Output kg/ m ².h | Moisture % |
|---|---|---|---|---|
| Iron concentrate | -200 mesh accounts for 52% | 45~65 | 500~1000 | 7~10 |
| Sulfur concentrate | -200 mesh accounts for 75% | 40~55 | 400~800 | 10~13 |
| Copper concentrate | -200 mesh accounts for 33% | 40~55 | 400~600 | 10~15 |
| Gold concentrate | -200 mesh accounts for 74% | 40~55 | 300~450 | 11~13 |
| Zinc concentrate | -200 mesh accounts for 99% | 45~55 | 500~700 | 12~13 |
| Phosphorus concentrate | -200 mesh accounts for 30% | 45~65 | 550~700 | 10~13 |
| Sulfur tailings | -400 mesh accounts for 92% | 45~55 | 300~400 | 13~15 |
| Cyanide slag | -325 mesh accounts for 83% | 40~55 | 350~550 | 25~27 |
| Iron tailings | -200 mesh accounts for 83% | 45~55 | 350~600 | 11~13 |
| Copper tailings | -400 mesh accounts for 90% | 45~55 | 350~450 | 11~15 |
| Molybdenum tailings | -200 mesh accounts for 80% | 50~55 | 350~450 | 12~15 |
| Phosphorus tailings | -400 mesh accounts for 80% | 50~60 | 350~700 | 12~15 |
| Quartz sand tailings | -200 mesh accounts for 80% | 40~55 | 300~350 | 14~15 |